Foundry Ceramic Sand, technically named as “Sintered Ceramic Sand for Foundry”, also named as ceramsite, cerabeads, ceramcast, some countries is also named Golden Sand, is good artificial spherical grain shape which is made from calcined bauxite . Its main content is aluminum oxide and Silicon oxide. Ceramic sand, has much better properties than that of silica sand to gain a better performance in foundry. It has high refractoriness, little thermal expansion, good angular coefficient, excellent flowability, High resistance to wear, crush and thermal shock, high reclamation rate.
Babban Abun Sinadari | Al₂O₃≥53%, Fe₂O₃<4%, TiO₂<3%, SiO₂≤37% |
Siffar hatsi | Siffar |
Angular Coefficient | ≤1.1 |
Girman Juzu'i | 45μm -2000μm |
Refractoriness | ≥1800℃ |
Yawan yawa | 1.5-1.6 g/cm3 |
Thermal Fadada (RT-1200℃) | 4.5-6.5x10-6/k |
Launi | Yashi |
PH | 6.6-7.3 |
Ma'adinan Ma'adinai | Soft + Corundum |
Farashin Acid | <1 ml/50g |
LOI | 0.1% |
Kaist ceramic foundry sand is about half as light as zircon and chromite, is about third as light as fused ceramic sand. Compared to these natural sand and other foundry media (the material is able to turn out about twice the number of molds per unit weight). Kaist ceramic foundry sand can deliver mold and core packages with a range of benefits that include higher-strength sand casting packages, with high heat resistance, low thermal expansion, improved final part resolution and a smoother surface finish. It can also be handled very easily, saving labor and transfer power costs. However, the manufacturer recommends paying attention to the amount of binder addition.
A matsayin tsaka tsaki abu, KAIST yumbu yashi yana da amfani ga acid da alkali resins.
Ana iya amfani dashi ko'ina don yin simintin ƙarfe, simintin ƙarfe da simintin ƙarfe mara ƙarfe, kamar simintin kumfa da aka ɓace, yashi mai rufi, yashi guduro, akwatin babban sanyi, daidaitaccen simintin simintin, da bugu na 3D.
Za'a iya daidaita girman girman barbashi bisa ga buƙatun ku.
raga |
20 | 30 | 40 | 50 | 70 | 100 | 140 | 200 | 270 | Pan | Farashin AFS | |
μm |
850 | 600 | 425 | 300 | 212 | 150 | 106 | 75 | 53 | Pan | ||
Lambar | 20/40 | 15-40 | 30-55 | 15-35 | ≤5 | 20±5 | ||||||
30/50 | ≤1 | 25-35 | 35-50 | 15-25 | ≤10 | ≤1 | 30±5 | |||||
40/70 | ≤5 | 20-30 | 40-50 | 15-25 | ≤8 | ≤1 | 43±3 | |||||
70/40 | ≤5 | 15-25 | 40-50 | 20-30 | ≤10 | ≤2 | 46±3 | |||||
50/100 | ≤5 | 25-35 | 35-50 | 15-25 | ≤6 | ≤1 | 50±3 | |||||
100/50 | ≤5 | 15-25 | 35-50 | 25-35 | ≤10 | ≤1 | 55±3 | |||||
70/140 | ≤5 | 25-35 | 35-50 | 8-15 | ≤5 | ≤1 | 65±4 | |||||
140/70 | ≤5 | 15-35 | 35-50 | 20-25 | ≤8 | ≤2 | 70±5 | |||||
100/200 | ≤10 | 20-35 | 35-50 | 15-20 | ≤10 | ≤2 | 110±5 |